Structure safety is of utmost importance in modern days. Now- a- days ferrocement is gaining popularity as a
retrofitting material due to ease of its application and availability. The most critical location of failure in any structure is beam
column joint. The aim of this paper is to analyse the effect of retrofitting on beam column joint using ferrocement as a
retrofitting material. Square wire mesh and triangular wire mesh was used for retrofitting beam column joint.