This paper deals with the experimental study of concrete by partial replacement of fine aggregate with copper slag and
glass powder to increase the strength parameters such as compressive strength, split tensile strength, and flexural strengths of
the M30 concrete. Here the fine aggregate partially replaced by copper slag (CS) and glass powder (GP) in CC,10%,20%,30%, &
40%. by weight of fine aggregate. Mix design was prepared for M30 grade of concrete. By replacement of copper slag and glass
powder as fine aggregate we can reduce the digging of river sand or natural sand which effects the hydraulic structure stability
and as well as we can reduce the open land fill and environmental pollution with copper slag usage it in concrete. Graphs are
drawn strength vs